Temperature promoting is one of the most important inspected targets for MOLSIV.MOLSIV is just in the relaxing heat as absorbing water,although temperature promoting is the intuitionistic way to exam the adsorption capability of MOLSIV.some companies add the alkali to MOLSIV in persuit of much more temperature,thus which not only corrupt the aluminum frame but also increase itself the ratio of wearing powder,all of these will decrease the work-span of insulated glass.the nomal molecular sieve is made from synthesized zeolite and little binder,no alkali,which can absorb the moisture in air continuously and effectivly,keep the low dew point and make sure long work-span of insulated glass.
The nomal MOLSIV is made from synthesized zeolite and little binder,no alkali,which can absorb the moisture in air continuously and effectivly,keep the low dew point and make sure long work-span of insulated glass.so the high-quality insulated glass is base on the premise that use the good-quality MOLSIV.
Suggestions for inspecting way :
The ways for PH value :
1.making 20g sample and 20ml water mixed.
2.putting little liquor on PH test paper.
3.comparing the colour on PH test paper with standard card,then getting the value.
The comparative illustration between nomal molsiv and product with alkali
MOLSIV:
PH: 9-10 (alkalescence)
Original temparature promoting:35-60℃
Recycle temparature promoting:32-46℃
Influence to insulated glass:tally with national standard.
The product with alkali:
PH:12-14(strong alkalescence)
Original temparature promoting:30-90℃
Recycle temparature promoting:10-25℃
Influence to insulated glass:accelerating aluminum frame corruption,decreasing adsorption capability of MOLSIV.

『LBC Product』

『Other Product A』

『Other Product B』

『Experiment processing』

『Results』
Photo taken in real,maybe have litter difference with the true colour ,taking the real product as the fact